A D V A N C E D M A N U F A C T U R I N G

NASA’S ORION CREW

VEHICLE SPORTS

3D-PRINTED VENTS

Orion’s Exploration Flight Test 1 vehicle used

four additively manufactured vent assemblies

to equalize pressure between unpressurized

portions of the spacecraft and the external

environment.